DOMADIA™ Tokkin 350

DOMADIA™ Tokkin 350

DOMADIA™ Tokkin 350 – High-Strength, Corrosion-Resistant Cr-Ni-Mo Stainless Steel

DOMADIA™ Tokkin 350 is a premium chromium-nickel-molybdenum stainless steel developed for applications demanding exceptional strength, durability, and corrosion resistance. Supplied in solution heat-treated and annealed conditions, this alloy exhibits excellent workability and achieves high strength through a specialized heat treatment process. Not made in India.

Unlike conventional precipitation-hardening stainless steels, DOMADIA™ Tokkin 350 contains no Aluminum or No Titanium, ensuring superior weldability without compromising performance. AKA Aluminium Free Steel. Its high yield strength, fatigue resistance, and cyclic stress tolerance make it ideal for precision-engineered components requiring long operational life!

Key Advantages

  • Heat-Treatable High Strength
    Achieves maximum strength through dual-stage hardening: martensitic transformation followed by precipitation hardening.
  • Enhanced Corrosion and Oxidation Resistance
    Molybdenum addition provides elevated resistance in harsh environments.
  • Excellent Weldability
    Free from Al and Ti, ensuring clean welds with minimal cracking or brittleness.
  • Fatigue-Resistant Design
    Superior cyclic fatigue strength makes it ideal for mechanically dynamic applications.

 

 Mechanical Properties of DOMADIA™ Tokkin 350

 As Annealed / As Rolled (2B Finish)

All values are maximums for strength and minimums for elongation.

Thickness (mm)Tensile Strength (MPa)Yield Strength (MPa)Elongation (%)Hardness (HV)
0.039 – 0.051≤ 1393≤ 641≥ 9Negotiable*
0.052 – 0.127≤ 1372≤ 627≥ 10Negotiable*
0.128 – 0.254≤ 1351≤ 614≥ 12Negotiable*
0.255 – 0.508≤ 1331≤ 600≥ 14Negotiable*

🔹 After Age Hardening (SCT850 Treatment)

Values are minimums for strength and elongation.

Thickness (mm)Tensile Strength (MPa)Yield Strength (MPa)Elongation (%)Hardness (HV)
0.039 – 0.508≥ 1276≥ 10344 – 8Negotiable*

Physical Properties of DOMADIA™ Tokkin 350

Condition: Solution Heat-Treated and Annealed

PropertyValueUnit / Range
Density7.92g/cm³
Specific Heat461J/(kg·K)
Electrical Resistivity79μΩ·cm
Thermal Expansion15.2 × 10⁻⁶/K (in the range 25–100°C)
Thermal Conductivity15.4W/(m·K) at 100°C

Chemical Composition of DOMADIA™ Tokkin 350

All values in mass %

ElementContent (mass%)
C (Carbon)0.07 – 0.11
Si (Silicon)≤ 0.50
Mn (Manganese)0.50 – 1.25
P (Phosphorus)≤ 0.040
S (Sulfur)≤ 0.030
Cr (Chromium)16.00 – 17.00
Ni (Nickel)4.00 – 5.00
Mo (Molybdenum)2.50 – 3.25
Fe (Iron)Balance
Others (Nitrogen)0.07 – 0.13 (N)

Standards and Designations for DOMADIA™ Tokkin 350

Standard BodyDesignationDescription
       UNS       S35000     Unified Numbering System alloy designation
ASTMA693 (Type 633)Specification for precipitation-hardening stainless steel plate, sheet, and strip
AMS5548Aerospace specification for corrosion-resistant steel, sheet, strip, and plate, annealed
AISI633American Iron and Steel Institute equivalent

Applications of DOMADIA™ Tokkin 350

1. Bellows

Used in systems that require repeated flexing, such as vacuum seals or expansion joints. Tokkin 350’s excellent cyclic fatigue strength ensures long life and reliability, even in corrosive or high-temperature environments.

2. Diaphragms

Ideal for pressureregulation and sensorcomponents, where precision and durability are critical. The alloy’s elasticity and structural integrity under stress offer consistentmechanicalresponse over millions of cycles.

3. Valves & Actuated Valves

Perfect for fluidcontrolsystems that demand strength, corrosion resistance, and precision. Suitable for both static components and dynamicactuators, especially in HVAC, industrial automation, and aerospace.

4. Air Conditioning Components

Resists humidity, saltspray, and cyclic thermal load—essential for parts like springclips, valveplates, andcontrollevers that must maintain performance in fluctuating conditions.

5. Watch Parts

Provides non-magnetic, corrosion-resistant, and durableperformance in high-precision miniature mechanisms. Suitable for springs,gears,andregulators in mechanical and smart timepieces.

 

🛡️ Corrosion Resistance of DOMADIA™ Tokkin 350

DOMADIA™ Tokkin 350 exhibits a range of corrosion resistance levels depending on the chemical environment. Its molybdenum-enriched composition enhances performance, especially in oxidizing and chloride-containing media.

EnvironmentResistance RatingClassification
HumiditySExcellent
Sea WaterRRestricted (Not Recommended)
Salt Spray (NaCl)AGood
Sodium HydroxideBModerate
Hydrochloric AcidRRestricted
Acetic AcidBModerate
Phosphoric AcidRRestricted
Sulphuric AcidRRestricted
Nitric AcidAGood

Get the Right Fit

Not sure which material suits your application?
We help you match your performance requirements with the best fiber option from our high-tech portfolio.

Get in touch with us Today!

📩 Email: sales@domadia.com

📱 Call/WhatsApp: +91-9594066275

SHOP ONLINE

Error: Contact form not found.

Product categories
Products